Minimize Defects on SMT process. Better wetting on unique metal. Wide process window & disigned for PIP. Good printing on small apertures & improve interval printing property. Special additives reducing void rates (LVA, Low void additives).
Flux Classifiction | ROL0 |
Alloy | LFM-48 |
Alloy Metal | Sn-3.0Ag-0.5Cu |
Temperature | 217° – 220°C |
Flux | NH (LVA) |
Flux % | 11.5 |
Powder Size | 20-38µm |
Weight | 500g |
Jar/Reel/Catridge | Jar |